論文

Fracture-mechanics-based evaluation of failure limit on pre-cracked and hydrided Zircaloy-4 cladding tube under biaxial stress states

Li, F.; 三原 武; 宇田川 豊; 天谷 政樹

Journal of Nuclear Science and Technology, 57(6), p.633 - 645, 2020/06

 被引用回数:3 パーセンタイル:34.82(Nuclear Science & Technology)

To better understand the failure limit of fuel cladding during the pellet-cladding mechanical interaction (PCMI) phase of a reactivity-initiated accident (RIA), pre-cracked and hydrided cladding samples with base metal final heat-treatment status of cold worked (CW) and recrystallized (RX) were tested under biaxial stress conditions (axial to hoop strain ratios of 0 and 0.5). Displacement-controlled biaxial-expansion-due-to-compression (biaxial-EDC) tests were performed to obtain the hoop strain at failure (failure strain) of the samples. The conversion of the failure strains to J-integral at failure by finite-element analysis involving data of stress-relieved (SR) cladding specimens from our previous study revealed that the failure limit in the dimension of J-integral at failure unifies the effects of pre-crack depth. About 30 to 50 percent reduction in the J-integral at failure was observed as the strain ratio increased from 0 to 0.5 irrespective of the annealing type, pre-crack depth, and hydrogen content. the rate of fractional decreases of J-integral at failure with increase of hydrogen content are in the order of CW$$>$$SR$$>$$RX, which are essentially independent of strain ratio for the CW and SR samples. The results were incorporated into the failure prediction model of the JAEA's fuel performance code in the form of a correction factor that considers the biaxial loading effect.

報告書

EDC試験手法による反応度事故時の燃料被覆管破損に及ぼす水素化物偏在及び2軸応力状態の影響の評価

篠崎 崇; 三原 武; 宇田川 豊; 杉山 智之; 天谷 政樹

JAEA-Research 2014-025, 34 Pages, 2014/12

JAEA-Research-2014-025.pdf:6.05MB

EDC(Expansion-Due-to-Compression)試験は、燃料被覆管の機械特性試験の一手法であり、反応度事故(RIA)時におけるペレット-被覆管機械的相互作用(PCMI)に着目した試験手法である。本研究では、高燃焼度燃料被覆管に見られる"水素化物リム"を模擬するために外周部に水素化物を偏析させた未照射被覆管を使用し、高燃焼度燃料のRIA時に被覆管に負荷される機械的条件を模擬したEDC試験を実施した。試料の水素濃度および偏析した水素化物の厚みが増加すると、試験後試料の周方向残留ひずみが低下する傾向が見られた。また、RIA時に被覆管外面の水素化物に発生するき裂を模擬するため、外面に予き裂を有する被覆管(RAG管)を作製し、この試料を対象としたEDC試験を行った結果、試料の予き裂深さが増加するにつれて破損時の周方向全ひずみが低下する傾向が見られた。さらに、RAG管試料に軸方向引張荷重を負荷することで2軸応力状態とし、EDC試験を実施した。このような2軸応力状態では、単軸引張条件である通常のEDC試験と比較して破損時の周方向全ひずみが低下する傾向が見られた。